Relationship between Yield Point Phenomena and the Nanoindentation Pop-in Behavior of Steel...

by T.-h. Ahn, C.-s. Oh, K. Lee, Easo P George, H. Han
Publication Type
Journal
Journal Name
Journal of Materials Research
Publication Date
Page Numbers
39 to 44
Volume
27
Issue
1